Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.450 - 44.2 GPa | 65.3 - 6410 ksi | Average value: 8.04 GPa Grade Count:181 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |