Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.20 - 4.30 GPa @Temperature 60.0 - 120 °C |
464 - 624 ksi @Temperature 140 - 248 °F |
Average value: 3.70 GPa Grade Count:1 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 2.30 - 4.30 GPa | 334 - 624 ksi | ASTM D638 |
Zeus PEEK Tubing PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used.. |