Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 36.5 - 40.0 GPa | 5290 - 5800 ksi | |
Ceradyne Thermo-Sil® UHS Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Modulus of Elasticity | 6.00 - 40.0 GPa | 870 - 5800 ksi | Average value: 14.7 GPa Grade Count:36 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |