Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.40 - 3.40 GPa @Temperature 60.0 - 120 °C |
348 - 493 ksi @Temperature 140 - 248 °F |
Average value: 2.87 GPa Grade Count:1 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Modulus of Elasticity | 0.00650 - 3.40 GPa | 0.943 - 493 ksi | Average value: 1.65 GPa Grade Count:22 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 3.30 - 3.40 GPa @Temperature 80.0 - 80.0 °C |
479 - 493 ksi @Temperature 176 - 176 °F |
Average value: 3.37 GPa Grade Count:3 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |