Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.79 - 3.24 GPa | 260 - 470 ksi | Average value: 2.37 GPa Grade Count:27 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Modulus of Elasticity | 0.00163 - 3.24 GPa | 0.237 - 470 ksi | Average value: 2.12 GPa Grade Count:55 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |