Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.50 - 31.8 GPa | 798 - 4610 ksi | Average value: 14.3 GPa Grade Count:46 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |