Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.50 - 29.0 GPa | 653 - 4200 ksi | Average value: 16.5 GPa Grade Count:8 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 1.60 - 29.0 GPa | 232 - 4200 ksi | Average value: 8.94 GPa Grade Count:55 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |