Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.65 - 2.88 GPa | 384 - 418 ksi | ASTM D638M |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Modulus of Elasticity | 2.65 - 2.88 GPa | 384 - 418 ksi | UV Postcure; ASTM D368M |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Modulus of Elasticity | 2.65 - 2.88 GPa | 384 - 418 ksi | ASTM D638M |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |