Mechanical Properties Metric English Comments
Modulus of Elasticity 8.27 - 28.3 GPa
1200 - 4100 ksi
Average value: 16.8 GPa Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Modulus of Elasticity 10.0 - 28.3 GPa
1450 - 4100 ksi
Average value: 20.0 GPa Grade Count:28
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..