Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.00 - 27.0 GPa @Temperature -40.0 - 250 °C |
870 - 3920 ksi @Temperature -40.0 - 482 °F |
Average value: 15.6 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Modulus of Elasticity | 6.00 - 27.0 GPa @Thickness 1.00 - 4.00 mm |
870 - 3920 ksi @Thickness 0.0394 - 0.157 in |
Average value: 15.6 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |