Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.50 - 26.5 GPa | 653 - 3840 ksi | Average value: 18.2 GPa Grade Count:34 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |