Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.00 - 2.65 GPa | 145 - 384 ksi | Average value: 2.09 GPa Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 2.37 - 2.65 GPa | 344 - 384 ksi | UV Postcure; ASTM D368M |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Modulus of Elasticity | 0.900 - 2.65 GPa | 131 - 384 ksi | Average value: 1.74 GPa Grade Count:36 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |