Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.80 - 22.8 GPa | 551 - 3300 ksi | Average value: 7.88 GPa Grade Count:23 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Modulus of Elasticity | 7.24 - 22.8 GPa | 1050 - 3300 ksi | Average value: 13.4 GPa Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |