Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.90 - 2.20 GPa @Temperature 60.0 - 90.0 °C |
276 - 319 ksi @Temperature 140 - 194 °F |
Average value: 2.05 GPa Grade Count:1 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 1.70 - 2.20 GPa @Temperature 60.0 - 120 °C |
247 - 319 ksi @Temperature 140 - 248 °F |
Average value: 1.93 GPa Grade Count:1 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 0.640 - 2.20 GPa @Temperature 60.0 - 150 °C |
92.8 - 319 ksi @Temperature 140 - 302 °F |
Average value: 1.21 GPa Grade Count:1 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Modulus of Elasticity | 0.200 - 2.20 GPa | 29.0 - 319 ksi | Average value: 1.02 GPa Grade Count:20 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 1.60 - 2.20 GPa | 232 - 319 ksi | Average value: 1.90 GPa Grade Count:7 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Modulus of Elasticity | 0.483 - 2.20 GPa | 70.1 - 319 ksi | Average value: 1.31 GPa Grade Count:3 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |