Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.000986 - 2.10 GPa | 0.143 - 305 ksi | Average value: 0.583 GPa Grade Count:31 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Modulus of Elasticity | 1.60 - 2.10 GPa @Temperature 60.0 - 120 °C |
232 - 305 ksi @Temperature 140 - 248 °F |
Average value: 1.83 GPa Grade Count:1 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |