Mechanical Properties Metric English Comments
Modulus of Elasticity 1.70 - 2.00 GPa
247 - 290 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_7230 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
Modulus of Elasticity 1.40 - 2.00 GPa
203 - 290 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Modulus of Elasticity 1.40 - 2.00 GPa
203 - 290 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Modulus of Elasticity 0.580 - 2.00 GPa

@Temperature 60.0 - 150 °C
84.1 - 290 ksi

@Temperature 140 - 302 °F
Average value: 1.10 GPa Grade Count:1
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Modulus of Elasticity 0.650 - 2.00 GPa

@Temperature 60.0 - 150 °C
94.3 - 290 ksi

@Temperature 140 - 302 °F
Average value: 1.15 GPa Grade Count:1
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Modulus of Elasticity 1.70 - 2.00 GPa
247 - 290 ksi
Biomer P226 PHB Biodegradable Polymer