Polymer Property : Modulus of Elasticity = 268 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.05 - 1.85 GPa
152 - 268 ksi
Average value: 1.59 GPa Grade Count:9
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..