Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 150 - 170 GPa | 21800 - 24700 ksi | Youngs Modulus |
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. Its machineability is one of the best of all of the corrosion resistant alloys. The very good machineability of.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H14 4/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C 0 Annealed, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H13 3/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H13 3/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H14 4/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H14 4/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1 H15 Spring, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C 0 Annealed, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H14 4/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1C H15 Spring, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 2.5< diameter< 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Modulus of Elasticity | 163 - 170 GPa | 23600 - 24700 ksi | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, diameter High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |