Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.14 - 15.4 GPa | 600 - 2230 ksi | Average value: 7.89 GPa Grade Count:34 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Modulus of Elasticity | 0.600 - 15.4 GPa @Temperature 60.0 - 175 °C |
87.0 - 2230 ksi @Temperature 140 - 347 °F |
Average value: 4.73 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |