Mechanical Properties Metric English Comments
Modulus of Elasticity 13.0 - 15.0 GPa
1890 - 2180 ksi
Injection; ISO 527
Raschig Group 2567 AMC
Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and ..
Modulus of Elasticity 13.0 - 15.0 GPa
1890 - 2180 ksi
Injection; ISO 527
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Modulus of Elasticity 13.0 - 15.0 GPa
1890 - 2180 ksi
Injection; ISO 527
Raschig Group 2572 AMC
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin..
Modulus of Elasticity 0.824 - 15.0 GPa
119 - 2180 ksi
Average value: 9.44 GPa Grade Count:182
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Modulus of Elasticity 2.28 - 15.0 GPa
331 - 2180 ksi
Average value: 9.02 GPa Grade Count:8
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 13.5 - 15.0 GPa

@Temperature 70.0 - 70.0 °C
1960 - 2180 ksi

@Temperature 158 - 158 °F
Average value: 10.1 GPa Grade Count:1
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Modulus of Elasticity 13.5 - 15.0 GPa

@Time 180000 - 1.44e+6 sec
1960 - 2180 ksi

@Time 50.0 - 400 hour
Average value: 10.1 GPa Grade Count:1
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Modulus of Elasticity 1.00 - 15.0 GPa
145 - 2180 ksi
Average value: 8.43 GPa Grade Count:471
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Modulus of Elasticity 1.00 - 15.0 GPa
145 - 2180 ksi
Average value: 7.98 GPa Grade Count:413
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Modulus of Elasticity 0.210 - 15.0 GPa
30.5 - 2180 ksi
Average value: 2.32 GPa Grade Count:128
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 2.25 - 15.0 GPa
326 - 2180 ksi
Average value: 6.31 GPa Grade Count:143
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Copyright © lookpolymers.com All Rights Reserved