Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.60 - 13.8 GPa | 957 - 2000 ksi | Average value: 11.5 GPa Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Modulus of Elasticity | 2.80 - 13.8 GPa | 406 - 2000 ksi | Average value: 7.28 GPa Grade Count:22 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Modulus of Elasticity | 0.930 - 13.8 GPa | 135 - 2000 ksi | Average value: 6.49 GPa Grade Count:74 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 2.41 - 13.8 GPa | 350 - 2000 ksi | Average value: 6.03 GPa Grade Count:86 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Modulus of Elasticity | 4.48 - 13.8 GPa | 650 - 2000 ksi | Average value: 6.61 GPa Grade Count:24 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 11.0 - 13.8 GPa | 1600 - 2000 ksi | Average value: 12.0 GPa Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |