Polymer Property : Modulus of Elasticity = 1700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.96 - 11.7 GPa
430 - 1700 ksi
Average value: 6.71 GPa Grade Count:14
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 3.45 - 11.7 GPa
500 - 1700 ksi
Average value: 7.36 GPa Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Modulus of Elasticity 3.00 - 11.7 GPa
435 - 1700 ksi
Average value: 6.79 GPa Grade Count:38
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 2.21 - 11.7 GPa
320 - 1700 ksi
Average value: 6.25 GPa Grade Count:9
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Modulus of Elasticity 10.3 - 11.7 GPa
1500 - 1700 ksi
ASTM D638
Premix Premi-Glas® 1200H-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..