Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.500 - 1.10 GPa @Temperature 60.0 - 90.0 °C |
72.5 - 160 ksi @Temperature 140 - 194 °F |
Average value: 0.800 GPa Grade Count:1 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Modulus of Elasticity | 0.510 - 1.10 GPa | 74.0 - 160 ksi | Average value: 0.702 GPa Grade Count:10 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 0.0200 - 1.10 GPa | 2.90 - 160 ksi | Average value: 0.678 GPa Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 0.650 - 1.10 GPa @Temperature 60.0 - 90.0 °C |
94.3 - 160 ksi @Temperature 140 - 194 °F |
Average value: 0.875 GPa Grade Count:1 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |