Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0320 - 1.00 GPa | 4.64 - 145 ksi | Average value: 0.302 GPa Grade Count:11 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |