Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.10 - 8.27 GPa | 305 - 1200 ksi | Average value: 5.57 GPa Grade Count:57 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Modulus of Elasticity | 0.00800 - 8.25 GPa | 1.16 - 1200 ksi | Average value: 1.76 GPa Grade Count:224 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 6.90 - 8.27 GPa | 1000 - 1200 ksi | Average value: 7.70 GPa Grade Count:6 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 4.14 - 8.27 GPa | 600 - 1200 ksi | Average value: 6.18 GPa Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |