Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0110 - 0.700 GPa | 1.60 - 102 ksi | Average value: 0.0939 GPa Grade Count:21 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 0.276 - 0.703 GPa | 40.0 - 102 ksi | ASTM D638M |
DSM Somos® 8120 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Modulus of Elasticity | 0.276 - 0.700 GPa | 40.0 - 102 ksi | Average value: 0.454 GPa Grade Count:8 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 0.343 - 0.700 GPa | 49.7 - 102 ksi | Average value: 0.378 GPa Grade Count:11 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |