Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 66.0 GPa | 9570 ksi | |
Schott AF 45 Thin Borosilicate Glass AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc.. |
|||
Modulus of Elasticity | 66.0 GPa | 9570 ksi | |
Schott Glass 8487 Borosilicate Glass Borosilicate glass for sealing to tungsten Backlights, flash lamps, lamp bulbs, exhaust and flare bulbs The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is .. |
|||
Modulus of Elasticity | 66.0 GPa | 9570 ksi | |
Schott Glass 8687 Borosilicate Glass Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |
|||
Modulus of Elasticity | 66.0 GPa | 9570 ksi | |
Schott KZFS12 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 66.0 GPa | 9570 ksi | |
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 66.0 GPa | 9570 ksi | |
Schott N-KZFS2 Glass Information Provided by SCHOTT North America, Inc. |