Mechanical Properties Metric English Comments
Modulus of Elasticity >= 0.650 GPa
>= 94.3 ksi
ISO 527-1
Orbilan ORBILAN® PE 1000 UHMW-PE
Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general mac..
Modulus of Elasticity 0.650 - 2.07 GPa
94.3 - 300 ksi
Average value: 1.26 GPa Grade Count:23
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Modulus of Elasticity 0.650 - 2.00 GPa

@Temperature 60.0 - 150 °C
94.3 - 290 ksi

@Temperature 140 - 302 °F
Average value: 1.15 GPa Grade Count:1
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Modulus of Elasticity 0.650 GPa
94.3 ksi
AorTech Biomaterials Elast-Eon™ E2-862 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Modulus of Elasticity 0.650 GPa
94.3 ksi
AorTech Biomaterials Elast-Eon™ E2-862 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Modulus of Elasticity 0.650 - 1.10 GPa

@Temperature 60.0 - 90.0 °C
94.3 - 160 ksi

@Temperature 140 - 194 °F
Average value: 0.875 GPa Grade Count:1
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Copyright © lookpolymers.com All Rights Reserved