Polymer Property : Modulus of Elasticity = 850 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 5.86 - 22.1 GPa
850 - 3200 ksi
Average value: 10.4 GPa Grade Count:21
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 5.86 - 20.0 GPa
850 - 2900 ksi
Average value: 11.6 GPa Grade Count:36
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Modulus of Elasticity 5.86 GPa
850 ksi
ASTM D638
ITW Devcon Plastic Steel® Metal Repair (A), Dark Grey
Information provided by ITW Devcon
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Devcon Plastic Steel® Liquid (B) Epoxy
General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a..
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Devcon Plastic Steel® Putty (A) Epoxy
General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. ..
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Devcon Wear Guard (Fine Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Devcon Wear Guard (High Temp) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Devcon Fastmeal™ Epoxy
Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m..
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Modulus of Elasticity 5.86 - 18.0 GPa
850 - 2610 ksi
Average value: 11.7 GPa Grade Count:17
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Modulus of Elasticity 5.86 - 9.00 GPa
850 - 1310 ksi
Average value: 8.07 GPa Grade Count:12
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..