Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 57.0 GPa | 8270 ksi | |
Schott F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 57.0 GPa | 8270 ksi | |
Schott F2HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 57.0 GPa | 8270 ksi | |
Schott SF56A Glass Information Provided by SCHOTT North America, Inc. |