Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 71.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.490 - 0.827 GPa
71.1 - 120 ksi
Average value: 0.654 GPa Grade Count:11
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..
Modulus of Elasticity 0.490 - 0.780 GPa
71.1 - 113 ksi
ASTM D638
Zeus EFEP Tubing
Modulus of Elasticity 0.490 - 0.780 GPa
71.1 - 113 ksi
ASTM D638
Zeus ETFE Tubing
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess..
Modulus of Elasticity 0.490 GPa
71.1 ksi
Film; DSM-Method, 50mm/min
DSM Akulon® XP32-E1 PA6
Film Extrusion, Medium Viscosity, Lubricated, Nucleated
Modulus of Elasticity 0.490 GPa
71.1 ksi
Film; DSM-Method, 50mm/min
DSM Akulon® XP36-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Modulus of Elasticity 0.490 GPa
71.1 ksi
Film; DSM-Method, 50mm/min
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Modulus of Elasticity 0.490 GPa
71.1 ksi
Film; DSM-Method, 50 mm/min
DSM Akulon® XP36-E1 PA6
Film Extrusion, Medium Viscosity, Nucleated, Lubricated
Modulus of Elasticity 0.490 GPa
71.1 ksi
Tangent; ASTM D790
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..