Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0517 - 0.293 GPa | 7.50 - 42.5 ksi | Average value: 0.176 GPa Grade Count:8 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Modulus of Elasticity | 0.0517 GPa | 7.50 ksi | ISO 1184-1983E |
LyondellBasell DP 8310M Polybutene Key Features: semi-crystalline high ethylene content random copolymerApplications: packaging industry, cast film, FDA acceptableMeets FDA requirements in 21 CFR 177.1570 for direct food contact up t.. |
|||
Modulus of Elasticity | 0.0517 GPa | 7.50 ksi | ISO 1184-1983E |
LyondellBasell DP 8510M Polybutene Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec.. |