Mechanical Properties Metric English Comments
Modulus of Elasticity 4.70 GPa
682 ksi
Conditioned; ISO 178
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 4.70 GPa
682 ksi
Conditioned; ISO 178
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 4.70 - 5.80 GPa

@Temperature 60.0 - 150 °C
682 - 841 ksi

@Temperature 140 - 302 °F
Average value: 5.30 GPa Grade Count:2
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Modulus of Elasticity 4.70 - 15.5 GPa

@Temperature 60.0 - 150 °C
682 - 2250 ksi

@Temperature 140 - 302 °F
Average value: 8.93 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..