Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.460 GPa | 66.7 ksi | film; DSM-Method, 50 mm/min |
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Modulus of Elasticity | 0.460 GPa | 66.7 ksi | film; DSM-Method, 50 mm/min |
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Modulus of Elasticity | 0.460 GPa | 66.7 ksi | ISO R527 |
Arkema Group Orgalloy® LT 5050 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Modulus of Elasticity | 0.460 GPa | 66.7 ksi | ISO R527 |
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |