Mechanical Properties Metric English Comments
Modulus of Elasticity 0.440 - 3.20 GPa
63.8 - 464 ksi
Average value: 1.66 GPa Grade Count:10
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 0.440 GPa
63.8 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i..
Modulus of Elasticity 0.440 GPa
63.8 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i..
Modulus of Elasticity 0.440 - 0.640 GPa
63.8 - 92.8 ksi
ASTM D638
Zeus FEP Tubing
FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua..
Modulus of Elasticity 0.440 GPa
63.8 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar® EZS is a high slip version of EZ. Used where a premium product appearance ..