Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.30 - 10.0 GPa | 624 - 1450 ksi | Average value: 6.97 GPa Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Modulus of Elasticity | 4.30 GPa | 624 ksi | |
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Modulus of Elasticity | 4.30 GPa | 624 ksi | ISO 527-1/-2 |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
Modulus of Elasticity | 4.30 GPa | 624 ksi | |
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |
|||
Modulus of Elasticity | 4.30 - 7.80 GPa @Temperature 60.0 - 120 °C |
624 - 1130 ksi @Temperature 140 - 248 °F |
Average value: 6.02 GPa Grade Count:2 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Modulus of Elasticity | 4.30 GPa | 624 ksi | |
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |
|||
Modulus of Elasticity | 4.30 - 11.5 GPa @Temperature 60.0 - 175 °C |
624 - 1670 ksi @Temperature 140 - 347 °F |
Average value: 6.88 GPa Grade Count:10 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |