Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.27 - 13.5 GPa | 620 - 1960 ksi | Average value: 10.5 GPa Grade Count:33 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |