Mechanical Properties Metric English Comments
Modulus of Elasticity 4.14 - 15.4 GPa
600 - 2230 ksi
Average value: 7.89 GPa Grade Count:34
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Modulus of Elasticity 4.14 - 24.1 GPa
600 - 3500 ksi
Average value: 10.1 GPa Grade Count:55
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Modulus of Elasticity 4.14 - 8.96 GPa
600 - 1300 ksi
Average value: 6.96 GPa Grade Count:13
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Modulus of Elasticity 4.14 GPa
600 ksi
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive..
Modulus of Elasticity 4.14 GPa
600 ksi
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive
AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive ..
Modulus of Elasticity 4.14 GPa
600 ksi
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive
AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati..
Modulus of Elasticity 4.14 - 8.27 GPa
600 - 1200 ksi
Average value: 6.18 GPa Grade Count:6
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..