Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0410 GPa | 5.95 ksi | ISO 527 |
Lucobit Lucobit® 1220 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Modulus of Elasticity | 0.0410 - 10.8 GPa | 5.95 - 1570 ksi | Average value: 3.93 GPa Grade Count:13 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |