Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 320 GPa | 46400 ksi | |
H.C. Starck HPM 1700 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
H.C. Starck HPM 1710 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | ASTM-F417 |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | ASTM-F417 |
CeramTec Alunit® HS Aluminum Nitride Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I.. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride Uniform, large sized pressed sintered aluminum nitride. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a.. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Ceradyne Ceralloy® 1370-1E Aluminum Nitride Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Ceradyne Ceralloy® 1370CS Aluminum Nitride Features:high thermal conductivityApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Ceradyne Ceralloy® 1370DP Aluminum Nitride Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Ceradyne Ceralloy® 147-5 Silicon Nitride Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's.. |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | |
Advanced Ceramics ACL 1085 (C-795) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Modulus of Elasticity | 320 GPa | 46400 ksi | ASTM-F417 |
CeramTec CeramCool® Alunit® Aluminum Nitride CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |