Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.013 - 12.5 GPa @Temperature -40.0 - 150 °C |
437.0 - 1810 ksi @Temperature -40.0 - 302 °F |
Average value: 6.79 GPa Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |