Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.76 GPa | 400 ksi | ASTM D638 |
Technetics Group Amicon™ Nylon 6/66
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Modulus of Elasticity | 2.76 - 7.50 GPa | 400 - 1090 ksi | Average value: 4.12 GPa Grade Count:4 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 2.76 - 15.2 GPa | 400 - 2200 ksi | Average value: 6.95 GPa Grade Count:59 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Modulus of Elasticity | 2.76 - 4.14 GPa | 400 - 600 ksi | Average value: 3.22 GPa Grade Count:6 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Modulus of Elasticity | 2.76 GPa | 400 ksi | Secant; ASTM D882 |
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating Parylene C is a polymer of para-xylylene modified by the substitution of a chlorine atom for one of the aromatic hydrogen atoms. Parylene C has a useful combination of electrical and physical proper.. |
|||
Modulus of Elasticity | 2.76 - 6.89 GPa | 400 - 999 ksi | |
ERG Aerospace Duocel® Silicon Carbide Foam Silicon Carbide (SiC) foam is a porous, open-celled structure made from an interconnected lattice of ceramic ligaments. The pattern of cells and ligaments repeats regularly throughout the entirety o.. |
|||
Modulus of Elasticity | 2.76 GPa | 400 ksi | IPC TM-650 2.4.18.3 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Modulus of Elasticity | 2.76 GPa | 400 ksi | ASTM D412 |
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets. |
|||
Modulus of Elasticity | 2.76 GPa | 400 ksi | ASTM D638 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Modulus of Elasticity | 2.76 GPa | 400 ksi | ASTM D882 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |
|||
Modulus of Elasticity | 2.76 - 5.52 GPa | 400 - 800 ksi | Average value: 4.21 GPa Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |