Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 26.5 GPa | 3840 ksi | ASMT D638 |
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent.. |