Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.65 - 2.88 GPa | 384 - 418 ksi | ASTM D638M |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Modulus of Elasticity | 2.65 - 17.9 GPa | 384 - 2600 ksi | Average value: 8.32 GPa Grade Count:124 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 2.65 - 2.88 GPa | 384 - 418 ksi | UV Postcure; ASTM D368M |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Modulus of Elasticity | 2.65 - 2.88 GPa | 384 - 418 ksi | ASTM D638M |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
Modulus of Elasticity | 2.65 - 7.58 GPa | 384 - 1100 ksi | Average value: 4.13 GPa Grade Count:16 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |