Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.495 GPa | 361.9 ksi | ASTM D638-04 |
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |