Mechanical Properties Metric English Comments
Modulus of Elasticity 0.248 GPa
36.0 ksi
Secant; ASTM D638
Huntsman PE1020 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 ..
Modulus of Elasticity 0.248 GPa
36.0 ksi
Secant; ASTM D638
Huntsman PE1041 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2..
Modulus of Elasticity 0.248 GPa
36.0 ksi
Molded Sample 2% Secant Modulus
Dow LDPE 5004IM Low Density Polyethylene
DOW LDPE 5004IM resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and rigidity with high ESCR. This resin has good processability over a wide range of..
Modulus of Elasticity 0.248 GPa
36.0 ksi
ASTM D638
Huntsman Rexell® L2101 Injection Molding LLDPE  (discontinued **)
Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,..
Modulus of Elasticity 0.248 GPa
36.0 ksi
Secant; ASTM D638
Huntsman PE2053 Injection Molding Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewar..