Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 240 GPa | 34800 ksi | |
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | |
H.C. Starck WCu 75/25 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | ASTM D3379-94 |
SGL Carbon Group SIGRAFIL C® C30 S003 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | ASTM D3379-95 |
SGL Carbon Group SIGRAFIL C® C30 S006 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | ASTM D3379-96 |
SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | ASTM D3379-97 |
SGL Carbon Group SIGRAFIL C® C30 S012 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | ASTM D3379-77 |
SGL Carbon Group SIGRAFIL C® C30 T050 EPY Continuous Tow Carbon Fiber with 50k filaments, Epoxy Sizing SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | ASTM D3379-78 |
SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | |
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | (hardened to 58 HRC) |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |
|||
Modulus of Elasticity | 240 GPa | 34800 ksi | |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |