Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 221 GPa | 32100 ksi | RT |
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | ASTM C848 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® 10V® (AISI A11) Tool Steel CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® S30V® Stainless Steel CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the form.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® S35VN™ Stainless Steel CPM S35VN is a martensitic stainless steel designed to offer improved toughness over CPM S30V. It is also easier to machine and polish than CPM S30V. Its chemistry has been rebalanced so that it for.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena.. |