Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 221 GPa | 32000 ksi | |
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi.. |
|||
Modulus of Elasticity | 221 GPa @Temperature 399 °C |
32000 ksi @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Modulus of Elasticity | 221 GPa | 32000 ksi | |
California Fine Wire Alloy 422 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Modulus of Elasticity | 221 GPa | 32000 ksi | |
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11) DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol.. |