Modulus of Elasticity 215 GPa

@Temperature 100 °C
31200 ksi

@Temperature 212 °F
Outokumpu 4016 Ferritic Stainless Steel
Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su..
Modulus of Elasticity 215 GPa
31200 ksi
RT
Outokumpu 4021 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Modulus of Elasticity 215 GPa
31200 ksi
RT
Outokumpu 4028 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Modulus of Elasticity 215 GPa
31200 ksi
Crucible Steel CPM® S90V® (420V®) Tool Steel
CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. ..
Modulus of Elasticity 215 GPa
31200 ksi
68°F, (hardened and tempered to 350 HB)
Bohler-Uddeholm BÖHLER RAMAX® HH Modified 420F
Chromium alloyed steelTypical applications for Ramax® HH are: holders and bolsters for plastic molds, plastic and rubber molds with low requirements on polishability, and dies for plastic extrusion..
Modulus of Elasticity 215 GPa
31200 ksi
(hardness of 40 HRC)
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel